Trends in Mechanical Engineering & Technology

Minimizing the Sand Casting Defects Using Taguchi Method

  1. Priyank V Parekh ✉
  2. J.A. Vadher

Abstract

The global market is becoming more and more quality conscious now a days. This Research work includes minimization of sand casting defects in C.I. based foundry. The survey was carried in small scale CI based foundry (Surat). Major defects were observed are misrun, coldshut, blowholes, and porosity. Taguchi method is used to optimize the control parameters like moisture, permeability, pouring time, pouring temperature. L18 orthogonal array is used in this research work. Critical parameters are optimized using Signal to noise Ratio (S/N Ratio). Cite this Article  Priyank V Parekh, Vadher JA. Minimizing the Sand Casting Defects Using Taguchi Method. Trends in Mechanical Engineering & Technology. 2016; 6(3): 14–17p

Keywords

References (6)

  1. Guharaja S, Noorul Haq Karuppannan K. Optimization of Green Sand Casting Process Parameters by using Taguchi’s method. Int J Adv Manuf Technol. October 2006; 30(11): 1040–1048p.
  2. Taguchi G. Taguchi on Robust Technology Development bringing Quality Upstream. ASME, New York, 1993.
  3. Sushil Kumar, Satsangi PS, Prajapati DR. Optimization of Green Sand Casting Process Parameters of a Foundry using Taguchi’s method. Int J Adv Manuf Technol. 2011; 55: 23–34p.
  4. Jain PL. Principles of Foundry Technology. McGraw-Hill, Second Reprint, 1996.
  5. Ross Phillip J. Taguchi Techniques for Quality Engineering . McGraw -Hill, Singapore, International Edition, 1996.
  6. Muzammil M, Pal Singh P, Talib F . Optimization of Gear Blank Casting Process by using Taguchi’s Robust Design Technique. J Qual Eng . 2003; 15: 351 – 359p. Cite this Article Priyank V Parekh, Vadher JA. Minimizing the Sand Casting Defects Using Taguchi Method. Trends in Mechanical Engineering & Technology . 2016; 6(3): 14–17p.

Read more of it

Subscribe to one journal or build your own list of several. One invoice, one payment, access for a full year.

Subscribe to journals →

Publish your article

Peer-reviewed journals across every subject, with open access options. Send your manuscript to the right editor today.

Publish with us → Calculate your APC
Support