Casting defects
5 articles · search the full text for this term
-
Injection Parameters Setting in High-Pressure Die Casting
Abstract: The advancement of science and processing technology is highly essential for the development of human civilization for a better life. Mass production leads to the availability of goods at a lesser price. Aluminium die-cast components are widely used in the automobile, aerospace, and consumer goods market. Proper process parameters are required to produce components with minimum rejections and scrap. This paper studies optimum injection parameters to produce components without defects. …
Published in Journal of Polymer & Composites · Vol. 11, Issue 13, 2023 · pp. 135–142 Read article
-
A Review on Study of Casting Defect in Automobile Component
Abstract: Casting process is the most widely used process in manufacturing industries especially in automotive products. Production of casting involves various processes like pattern making, molding, core making and melting. It is very difficult to produce defect free castings. In developing country, foundry industries suffer from poor quality and productivity due to involvement of number of process parameters in casting process, which challenges explanation about the cause of casting defects. The …
Published in Journal of Production Research & Management · Vol. 8, Issue 2, 2018 · pp. 8–13 Read article
-
A Review Paper on Minimisation of Sand Casting Defects through Quality Improvement Methods
Abstract: Casting is a process of producing near net–shape metal components. It requires detailed planning, execution and quality inspection to ensure not only the dimensional accuracy of casting parts but the metallurgical integrity and mechanical properties of castings. This paper reviews the different types of casting defects such as shrinkage porosity, cold shut, sand inclusions, mould failure, surface hardening occurring in foundries. These defects directly affect on profitability and quality level …
Published in Journal of Thin Films, Coating Science Technology & Application · Vol. 4, Issue 3, 2017 · pp. 10–17 Read article
-
Minimizing the Sand Casting Defects Using Taguchi Method
Abstract: The global market is becoming more and more quality conscious now a days. This Research work includes minimization of sand casting defects in C.I. based foundry. The survey was carried in small scale CI based foundry (Surat). Major defects were observed are misrun, coldshut, blowholes, and porosity. Taguchi method is used to optimize the control parameters like moisture, permeability, pouring time, pouring temperature. L18 orthogonal array is used in this …
Published in Trends in Mechanical Engineering & Technology · Vol. 6, Issue 3, 2016 · pp. 14–17 Read article
-
Optimization of Green Sand Casting Process Parameters by Artificial Neural Network
Abstract: In this paper, artificial neural network (ANN) is used to train the network which can predict the casting defect. L27 orthogonal array is used as input matrix for training of neural network. NN tool is used to train the network for prediction of defects. Major defects observed on shop floor were; misrun, blowholes, inclusions and porosity. Moisture, permeability, LOI, compressive strength, volatile content, vent holes, pouring time, pouring temperature, mould …
Published in Trends in Mechanical Engineering & Technology · Vol. 6, Issue 2, 2016 · pp. 75–80 Read article