3 publications

  • Published Subscription Original Research Special issue

    Study of Contact Temperature During Polishing of Zinc Plate with Ultrasonic Vibration Using Single Pole Magnetic Abrasive Finishing

    Abstract: The present work scrutinizes the impact of ultrasonic vibration on the contact temperature during polishing zinc plates with Single Pole Magnetic Abrasive Finishing (SPMAF). The efficacy and eminence of FMAB finishing are pointedly influenced by heat generation at the interaction point, as raised up temperatures can lead to the deprivation of abrasive elements or the bonding material inside the brush, which leads to the fading its overall effectiveness. The magnetic …

    Published in Journal of Polymer & Composites · Vol. 14, Issue 2, 2026 · pp. 1239–1247 Read article

  • Published Subscription Original Research Special issue

    Experimental Investigation into Surface Roughness of Polished Zinc Plate with Ultrasonic Vibration Using Single Pole Magnetic Abrasive Finishing

    Abstract: This research investigates how applying ultrasonic vibrations influences the surface finish quality of zinc plates when using the Single Pole Magnetic Abrasive Finishing (SP-MAF) method. In SP-MAF, magnetic abrasive particles (MAPs)—amalgamation of ferromagnetic and abrasive materials—are guided by a magnetic field to achieve precise surface finishing. Introducing ultrasonic vibration improves the effectiveness of the flexible magnetic abrasive brush (FMAB), which forms as the MAPs align along the magnetic field lines. …

    Published in Journal of Polymer & Composites · Vol. 14, Issue 2, 2026 · pp. 1166–1178 Read article

  • Published Subscription Original Research Special issue

    Study of pH Behaviour of Slurry on Surface Morphology of Copper Material with Single Pole Magnetic Abrasive Finishing Process

    Abstract: The chemical oxidizers—sodium hydroxide, Marshall’s acid salt, and hydrogen peroxide—were effectively employed in the wet polishing of copper using the SPMAF experimental setup. The manuscript explores preparation of slurry used for polishing copper material using single pole magnetic abrasive finishing (SPMAF) framework. The slurry contains distilled water, 1200-grit aluminum oxide abrasives, sodium hydroxide (NaOH), potassium persulfate (K₂S₂O₈), and hydrogen peroxide (H₂O₂), combined in precise amount. Specifically, 100 ml of distilled …

    Published in Journal of Polymer & Composites · Vol. 14, Issue 1, 2026 · pp. 1887–1896 Read article