Failure Analysis of Spur Pinion Tooth of Three Wheeler Gear Box
Abstract: In a gear, various types of damage can occur over a period of its operation. Therefore, it is necessary to establish some tools and techniques for finding failure causes related to the material. In this paper, all possible causes responsible for the spur pinion tooth failure are enlisted and procedures for testing various mechanical properties, chemical compositions are explained. The main objective of this work was aimed at to know …
Published in Journal of Automobile Engineering and Applications · Vol. 1, Issue 1, 2014 · pp. 1–5 Read article
-
An Assessment of Interfacial Chemistry and Character of Fiber/Polymer Microcomposites
Abstract: AbstractThe interfacial chemistry and character of hygrothermally treated E-glass/epoxy microcomposite have been investigated by Fourier transform infrared spectroscope (FTIR-imaging), temperature-modulated differential scanning calorimeter (TMDSC) and scanning electron microscope (SEM) techniques. The physico-chemical interactions occurring between absorbed water molecules and the network of a tetrafunctional epoxy resin were studied by FTIR-imaging. This is used to study the mechanistic details of epoxy curing on the molecular level. Absorbance peaks of OH stretching …
Published in Journal of Polymer & Composites · Vol. 1, Issue 1, 2013 · pp. 1–5 Read article
-
E-glass Fiber Epoxy Composites: Role of Al2O3/SiC Fillers in Physical, Flammability and Mechanical Characteristics
Abstract: This study investigates the effects of varying weight percentages of Silicon Carbide and Alumina particles in epoxy-based composites, fabricated through compression molding, on their physical and mechanical properties. Comparing different studies on carbon fiber-reinforced polymer (CFRP) composites, as well as glass fiber-reinforced polymer (GFRP) composites, especially with the reinforcement of nanoparticles such as silicon carbide (SiC), alumina (Al2O3) and graphene. The investigations cover fabrication methods, like vacuum infusion and compression …
Published in Journal of Polymer & Composites · Vol. 13, Issue 1, 2025 · pp. 238–250 Read article
-
Effects of Composition on Structure & Mechanical Property of TiAl Based Intermetallic Compounds
Abstract: The effects of Al content and ternary additions such as Mo, V and Si in as cast g based alloys made by plasma arc melting on solidification structures and mechanical properties were studied. The Columnar g /a2 lamellar structures in Al-lean alloys due to primary a solidification had higher room temperature fracture strength and strain than g phase structures through the reaction of L + a = g in Al-rich …
Published in Journal of Materials & Metallurgical Engineering · Vol. 11, Issue 3, 2021 · pp. 1–10 Read article
-
Study on High Strength Ti-Al-V Alloy at Cryogenic Temperature
Abstract: The α+β type high strength titanium alloy is usually used as a structural biomaterial for the manufacturing of orthopaedic prostheses as well as surgical and dental implants. The Ti-Al-V alloy had been deliberately solution treated at 860°C for 1 h (subsequently quenched in variable mediums) just below the β transus but within the α+β region to avoid grain coarsening for single β region as well as accomplish optimum balance properties …
Published in Journal of Materials & Metallurgical Engineering · Vol. 13, Issue 1, 2023 · pp. 1–14 Read article
-
Microstructural and Mechanical responses of Al6061 alloy matrix composite reinforced with yttria particles
Abstract: The increasing need for materials that can improve the overall performance of automotive and aerospace components has driven the development of composite materials. Aluminium Metal Matrix Composites (AMMC) have become a popular alternative due to their ability to satisfy the changing needs of industries. This study investigates the mechanical characteristics of AMMC (Aluminium Matrix Metal Composite) made using the stir casting method. The study examines the effects of different amounts …
Published in Journal of Polymer & Composites · Vol. 12, Issue 2, 2024 · pp. 246–252 Read article
-
Experimental Investigation of Hardness of FSW Al 5083 Alloy for Naval and Marine Application
Abstract: Friction stir welding (FSW) is a relatively novel method of solid-state joining. This connecting method is adaptable, environmentally benign, and low-energy. The present study focuses on hardness testing on welded butt joints, introducing the Friction Stir Welding procedure on aluminium alloys Al 5083, which are known for their remarkable performance in severe conditions. It is widely used in naval and marine applications due to its excellent resistance to seawater damage. …
Published in Journal of Polymer & Composites · Vol. 12, Issue 1, 2024 · pp. 227–236 Read article