Nano-mechanical and viscoelastic behavior of advance ultrafine graphite reinforced unsaturated polyester based prosthesis layup resin
Abstract: A new durable biomedical composite for prosthesis was designed to obtain enhance mechanical and viscoelastic properties, in particular nanohardness and young’s modulus. The nanoindentation technique was employed to investigate nano-scale mechanical properties of unsaturated polyester resin and its advance prosthesis lay-up nanocomposite resin with different amount of exfoliated graphite fillers loading. It has been observed that the young’s modulus of the nanocomposites gradually increase with increasing amount of reinforcement content. …
Published in Journal of Thin Films, Coating Science Technology & Application · Vol. 7, Issue 2, 2020 · pp. 7–15 Read article