Failure Analysis of Spur Pinion Tooth of Three Wheeler Gear Box
Abstract: In a gear, various types of damage can occur over a period of its operation. Therefore, it is necessary to establish some tools and techniques for finding failure causes related to the material. In this paper, all possible causes responsible for the spur pinion tooth failure are enlisted and procedures for testing various mechanical properties, chemical compositions are explained. The main objective of this work was aimed at to know …
Published in Journal of Automobile Engineering and Applications · Vol. 1, Issue 1, 2014 · pp. 1–5 Read article