International Journal of Industrial and Product Design Engineering Review Article

Evaluation of Critical MMAW Welding Defects Using Computer Simulation in Industrial Manufacturing Systems

  1. Sindhu Kumar Department of Mechanical engineering, EIT, Faridabad
  2. Rone Department of Mechanical engineering, EIT, Faridabad
  3. Manish Kumar Department of Mechanical engineering, EIT, Faridabad

Abstract

Manufacturing is one of the key sectors of any countries GDP and welding is one of the prime manufacturing processes of the manufacturing sector. Welding has several notable advantages over mechanical joining techniques, including higher structural integrity, design flexibility, and cost and weight lowers. Welded products/structures are subjected to serious issues of residual stresses and distortions. The performance and sturdiness of the welded structures are severely impacted by weld remaining strain and deformation. Welding distortions introduce sever problems in assembling of the welded structures and reduce its quality. In some cases the higher values of the distortions make the products useless in shape. Whereas, the residual stresses cause the premature failures of the structures during the service life. Hence there is a need for suitable a methodology to control/minimize the residual stresses and distortions. Accordingly, this study has proposed three distinct methods, namely pre- setting, restraining and auxiliary side heating to control distortion in butt welds of MMAW process. Similarly auxiliary side heating is also proposed to control the residual stresses. For pre-setting the workpieces with known magnitudes of angular distortion in the opposite direction, a linear regression model based on five independent process parameters/factors (current, welding speed, electrode diameter, number of passes and plate thickness) is developed to predict the magnitude of angular distortion. The efficiency of linear regression model is tested through confirmation tests and it is found that a variation of the predicted angular distortion is within 10%. Similar to the regression model, use of Finite Element Analysis (FEA) is made for predicting angular distortion and residual stresses.

Keywords

References (30)

  1. Aarbogh H.M.,, Hamide M., Fajer H.G., Mo A., Bellet M., Experimental validation of finite element codes for welding deformations, Journal of Materials Processing Technology, 210, (2010), 1681–1689.
  2. Abdulkareem S. Aloraier and Suraj Joshi, Residual stresses in flux cored arc welding process in bead-on-plate specimens, Materials Science and Engineering A,534, (2012),13–21.
  3. Abid M and Qarni M J, Numerical investigation of residual stresses and distortions due to multi-pass welding in a pipe-flange joint, IMechE Vol. 224 Part E: J. Process Mechanical Engineering, (2010), 253–267.
  4. Abid M. and Siddique M., Numerical simulation to study the effect of tack welds and root gap on welding deformations and residual stresses of a pipe-flange joint, International Journal of Pressure Vessels and Piping, 82, (2005), 860–871.
  5. Adak M. and Mandal N.R., Pseudolinear equivalent constant rigidity concept for analysing welding residual deformation, Applied Mathematical Modelling, 33 (2009), 2096–2108.
  6. Adak M., Mandal N.R., Numerical and experimental study of mitigation of welding distortion, Applied Mathematical Modelling, 34, (2010), 146–158.
  7. Ahmadzadeh M., HoseiniFard A., Saranjam B. and Salimi H.R., Prediction of residual stresses in gas arc welding by back propagation neural network, NDT&E International, 52, (2012), 136–143.
  8. Akbari and Sattari-Far I., Effect of the welding heat input on residual stresses in butt-welds of dissimilar pipe joints, International Journal of Pressure Vessels and Piping, 86, (2009),769–776.
  9. ALFARO S.C.A, MODENESI P.J. and SCOTTI A., The Use of Statistical Modelling in Welding, Journal of Materials Processing Technology, 38, (1993) 399–406.
  10. Anawa M. and Olabi A.G., Control of welding residual stress for dissimilar laser welded materials, Journal of Materials Processing Technology 204 (2008) 22–33.
  11. Andrés Anca, Alberto Cardona, José Risso and Víctor D. Fachinotti, Finite element modeling of welding processes, Applied Mathematical Modelling,35, (2011), 688–707.
  12. ANSYS 14.0 User's documentation, SAS IPInc, Canonburg, 2005, PA15317, USA,.
  13. Armentani , Esposito R. and Sepe R., The effect of thermal properties and weld efficiency on residual stresses in welding, Journal of Achievements in Materials and Manufacturing Engineering, Volume 20, Issues 1–2 Jan-Feb 2007,319–322.
  14. AsleZaeem M., Nami M.R., Kadivar M.H., Prediction of welding buckling distortion in a thin wall aluminium T joint, Computational Materials Science, 38, (2007), 588–594.
  15. ASM Metals Handbook Volume 2-Properties and Selection Nonferrous Alloys and Special Purpose Materials, ASM International, ISBN 0-87170-378-5 (Vol-II).
  16. Bae Y. and Na S.J., An analysis of thermal stress and distortion in bead-on-plate welding using laminated isotropic plate theory, Journal of Materials Processing Technology, 57, (1996), 337–344.
  17. Barroso A., Cañas J., Picón R., París F., Méndez C. and Unanue I., Prediction of welding residual stresses and displacements by simplified models. Experimental validation, Materials and Design, 31, (2010), 1338–1349.
  18. Barsoum Z. and Lundbäck A., Simplified FE welding simulation of fillet welds – 3D effects on the formation residual stresses, Engineering Failure Analysis,16 (2009), 2281–2289.
  19. Bart O. Nnaji, Deepak Gupta, Kyoung-Yun Kim, Welding Distortion Minimization for an Aluminium Alloy Extruded Beam Structure Using a 2D Model, ASME Journal of Manufacturing Science and Engineering, Vol. 126, (2004), 52–63.
  20. Bergheau, J. M., Contributions of numerical modelling to the optimization of welding processes', Welding International, 19: 12,(2005), 956 –966.
  21. Biswas P and Mandal N R, Thermomechanical finite element analysis and experimental investigation of single-pass single-sided submerged arc welding of C–Mn steel plates, Proc. IMechE Vol. 224 Part B: J. Engineering Manufacture, (2009),627–639.
  22. Biswas P, Mahapatra M and Mandal N R, Numerical and experimental study on prediction of thermal history and residual deformation of double-sided fillet welding, (2009),125–134.
  23. Biswas P., Mandal N.R., and Sha O.P., Three-dimensional finite element prediction of transient thermal history and residual deformation due to line heating, Proc. IMechE Vol. 221 Part M: J. Engineering for the Maritime Environment, (2007),17–30.
  24. Brickstad B. and Josefsonb B.L., A parametric study of residual stresses in multi- pass butt-welded stainless steel pipes, International Journal of Pressure Vessels and Piping, 75, (1998), 1 l–25.
  25. Brown T.B., Dauda T.A., Truman C.E., Smith D.J., Memhard D. and Pfeiffer, Predictions W. and measurements of residual stress in repair welds in plates, International Journal of Pressure Vessels and Piping, 83 (2006), 809–818.
  26. Buschenhenke F., Hofmann M., Seefeld T.and Vollertsen F., Distortion and residual stresses in laser beam weld shaft-hub joints, Physics Procedia, 5, (2010), 89–98.
  27. Camilleri D, Mollicone P, and Gray T G F, Computational methods and experimental validation of welding distortion models, Proc. IMechE Vol. 221 Part L:J. Materials: Design and Applications, (2007),235–249
  28. Camilleri D., Mollicone P., and Gray T G F, Computational prediction of out-of- plane welding distortion and experimental investigation, Journal of Strain Analysis ,Vol. 40 No. 2, (2005),161–176.
  29. Capriccioli Andrea and Paolo Frosi, Multipurpose ANSYS FE procedure for welding processes simulation, Fusion Engineering and Design, 84, (2009), 546–
  30. Casalino G, Hu S J and Hou W, Deformation prediction and quality evaluation of the gas metal arc welding butt weld, Proc. Instn Mech. Engrs Vol. 217 Part B: Engineering Manufacture, (2003), 1615–1622.
Support